The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 09, 2017

Filed:

Jun. 26, 2014
Applicant:

Exxonmobil Chemical Patents Inc., Baytown, TX (US);

Inventors:

Peijun Jiang, League City, TX (US);

Armenag Dekmezian, Austin, TX (US);

Aspy K. Mehta, Humble, TX (US);

Sunny Jacob, Seabrook, TX (US);

Andrew G. Narvaez, Jr., League City, TX (US);

Pradeep P. Shirodkar, Houston, TX (US);

Weiqing Weng, Houston, TX (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 23/00 (2006.01); C08L 47/00 (2006.01); C08L 23/12 (2006.01); C08L 23/14 (2006.01); C08F 210/06 (2006.01); C08L 23/10 (2006.01); C08L 23/16 (2006.01); C08F 110/06 (2006.01); C08L 23/04 (2006.01); C08L 23/08 (2006.01); C08L 91/00 (2006.01);
U.S. Cl.
CPC ...
C08L 47/00 (2013.01); C08F 210/06 (2013.01); C08L 23/10 (2013.01); C08L 23/12 (2013.01); C08L 23/14 (2013.01); C08L 23/145 (2013.01); C08L 23/16 (2013.01); C08F 110/06 (2013.01); C08L 23/04 (2013.01); C08L 23/083 (2013.01); C08L 91/00 (2013.01); C08L 2205/03 (2013.01); C08L 2205/22 (2013.01); C08L 2207/02 (2013.01); C08L 2308/00 (2013.01); C08L 2312/00 (2013.01);
Abstract

A heterogeneous in-situ polymer blend comprising a continuous phase comprising a polypropylene having a crystallinity of at least 30% and a melting point temperature Tgreater than 130° C., and a heat of fusion ΔHgreater than 65 J/g; and a dispersed phase comprising particles of an elastomeric copolymer dispersed in the continuous phase and having an average particle size of less than 5 micron, the elastomeric copolymer comprising ethylene units and 0.001 to 5 wt % diene by weight of the copolymer, and having a crystallinity of less than 20% and being at least partially cross-linked such that the degree of cross-link is at least 20%.


Find Patent Forward Citations