The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 09, 2017

Filed:

Dec. 20, 2005
Applicants:

Dennis Stamires, Dana Point, CA (US);

Paul O'connor, Hoevelaken, NL;

Erik Jeroen Laheij, Amstelveen, NL;

Charles Vadovic, Houston, TX (US);

Inventors:

Dennis Stamires, Dana Point, CA (US);

Paul O'Connor, Hoevelaken, NL;

Erik Jeroen Laheij, Amstelveen, NL;

Charles Vadovic, Houston, TX (US);

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B01J 29/08 (2006.01); B01D 53/94 (2006.01); B01J 29/06 (2006.01); B01J 37/00 (2006.01); C01B 3/02 (2006.01); C10G 1/08 (2006.01); C10G 2/00 (2006.01); C10G 11/05 (2006.01); C10G 29/20 (2006.01); C10G 35/06 (2006.01); C10G 49/08 (2006.01); B01J 35/00 (2006.01);
U.S. Cl.
CPC ...
B01J 29/084 (2013.01); B01D 53/94 (2013.01); B01J 29/06 (2013.01); B01J 37/0045 (2013.01); C01B 3/02 (2013.01); C10G 1/086 (2013.01); C10G 2/33 (2013.01); C10G 11/05 (2013.01); C10G 29/205 (2013.01); C10G 35/06 (2013.01); C10G 49/08 (2013.01); B01J 35/002 (2013.01); B01J 2229/42 (2013.01); C01B 2203/1041 (2013.01);
Abstract

A process for preparing a catalyst is disclosed. The process generally comprises the steps of: (a) preparing a slurry comprising clay, zeolite, a sodium-free silica source, quasi-crystalline boehmite, and micro-crystalline boehmite, provided that the slurry does not comprise peptized quasi-crystalline boehmite; (b) adding a monovalent acid to the slurry; (c) adjusting the pH of the slurry to a value above about 3, and (d) shaping the slurry to form particles. This process results in attrition resistant catalysts with a good accessibility.