The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 02, 2017

Filed:

Jul. 17, 2015
Applicant:

Sun Chemical Corporation, Parsippany, NJ (US);

Inventors:

Steven Johnson, Fairfield, OH (US);

John Nimmo, Kent, GB;

Mike Venturini, Macungie, PA (US);

Assignee:

Sun Chemical Corporation, Parsippany, NJ (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 9/06 (2006.01); C08F 136/08 (2006.01); C08F 36/06 (2006.01); C08F 36/04 (2006.01); C08L 7/00 (2006.01); C08L 23/16 (2006.01); C08L 61/00 (2006.01); C09D 119/00 (2006.01); C09D 121/00 (2006.01); C08L 61/06 (2006.01); C08L 77/00 (2006.01); C09D 161/06 (2006.01); C09D 177/00 (2006.01);
U.S. Cl.
CPC ...
C08L 9/06 (2013.01); C08F 36/04 (2013.01); C08F 36/06 (2013.01); C08F 136/08 (2013.01); C08L 7/00 (2013.01); C08L 23/16 (2013.01); C08L 61/00 (2013.01); C08L 61/06 (2013.01); C08L 77/00 (2013.01); C09D 119/003 (2013.01); C09D 121/00 (2013.01); C09D 161/06 (2013.01); C09D 177/00 (2013.01); C08K 2201/003 (2013.01); C08K 2201/005 (2013.01);
Abstract

A pigment and method for making a pigment comprising a milled elastomer, wherein the milled elastomer has a D50 particle size of between about 5 and about 50 microns. A coating of the pigment has a smoothness of about 3 or less. The pigment is prepared by providing an elastomer; and milling the elastomer in the presence of milling media and solvent at a temperature from about 30° C. to about 70° C. The elastomer is insoluble in the solvent. The method for preparing the pigment from an elastomer comprises the steps of: providing an elastomer; and milling the elastomer in a media mill in the presence of milling media and solvent at a temperature from about 30° C. to about 70° C. The diameter of the milling media is from about 0.5 mm to about 10 mm, and the elastomer is insoluble in the solvent.