The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 02, 2017

Filed:

Oct. 08, 2013
Applicant:

Basf SE, Ludwigshafen, DE;

Inventors:

Theodore M. Smiecinski, Woodhaven, MI (US);

Chad Alan Rogers, Dimondale, MI (US);

Assignee:

BASF SE, Ludwigshafen, DE;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G 18/76 (2006.01); C08G 18/48 (2006.01); C08G 18/66 (2006.01); C08G 18/32 (2006.01); C08G 18/08 (2006.01); C08G 18/61 (2006.01); C08G 101/00 (2006.01);
U.S. Cl.
CPC ...
C08G 18/7621 (2013.01); C08G 18/14 (2013.01); C08G 18/3275 (2013.01); C08G 18/4812 (2013.01); C08G 18/4829 (2013.01); C08G 18/4841 (2013.01); C08G 18/4845 (2013.01); C08G 18/61 (2013.01); C08G 18/6688 (2013.01); C08G 2101/0008 (2013.01); C08G 2101/0058 (2013.01); C08G 2101/0083 (2013.01);
Abstract

The subject disclosure provides a viscoelastic polyurethane foam and a method of forming the viscoelastic polyurethane foam. The viscoelastic polyurethane foam comprises the reaction product of a toluene diisocyanate and an isocyanate reactive component. The isocyanate reactive component comprises a first polyether triol, a second polyether triol, an amino alcohol chain extender, and a hydrolyzable polyether polydimethylsiloxane copolymer. The first polyether triol has a weight-average molecular weight of from 500 to 5,000 g/mol, at least 60 parts by weight ethyleneoxy units, based on the total weight of the first polyether triol, and at least 10% ethyleneoxy end caps. The second polyether triol, which is different from the first polyether triol, has a weight-average molecular weight of from 5,000 to 10,000 g/mol and at least 80% ethyleneoxy end caps.


Find Patent Forward Citations

Loading…