The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 18, 2017

Filed:

Dec. 26, 2014
Applicant:

Kuraray Co., Ltd., Kurashiki-shi, JP;

Inventors:

Hiroshi Ozawa, Tainai, JP;

Yasuhito Kitade, Tainai, JP;

Shouji Tanaka, Tainai, JP;

Assignee:

KURARAY Co., Ltd., Kurashiki-shi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08F 220/14 (2006.01); C08F 20/14 (2006.01); C08F 2/02 (2006.01); C08F 120/14 (2006.01); B01J 19/18 (2006.01);
U.S. Cl.
CPC ...
C08F 220/14 (2013.01); C08F 120/14 (2013.01); C08F 2400/02 (2013.01);
Abstract

A method for producing a (meth)acrylic resin composition, the method comprises the steps of continuously feeding methyl methacrylate and the other materials into a tank reactor while controlling each of the amounts thereof, performing bulk polymerization in the tank reactor to obtain a reaction product, recovering a mixture (A) containing methyl methacrylate and the others from the reaction product, and continuously feeding the mixture (A) into the tank reactor, wherein each of the amounts of methyl methacrylate and the others being fed into the tank reactor are controlled on the basis of the amount of the mixture (A) being fed into the tank reactor and the proportions of methyl methacrylate and the others in the mixture (A), and the perfect-mixing time of the tank reactor, the half life of a radical polymerization initiator at a temperature equal to the temperature inside the tank reactor, the agitation power of the tank reactor, the mean residence time of a reaction starting material in the tank reactor, and the concentration of the radical polymerization initiator in the reaction starting material satisfy a particular relationship.