The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Apr. 18, 2017

Filed:

Sep. 04, 2014
Applicant:

Matsuura Machinery Corporation, Fukui, Fukui, JP;

Inventors:

Koichi Amaya, Fukui, JP;

Toshihiko Katoh, Fukui, JP;

Hideto Matsubara, Fukui, JP;

Mitsuyoshi Yoshida, Fukui, JP;

Assignee:

Matsuura Machinery Corporation, Fukui, Fukui, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B23K 15/00 (2006.01); B22F 3/10 (2006.01); B22F 3/105 (2006.01); B33Y 30/00 (2015.01); B29C 67/00 (2017.01);
U.S. Cl.
CPC ...
B23K 15/0086 (2013.01); B22F 3/1017 (2013.01); B22F 3/1028 (2013.01); B22F 3/1055 (2013.01); B22F 2003/1056 (2013.01); B29C 67/0077 (2013.01); B33Y 30/00 (2014.12); Y02P 10/295 (2015.11);
Abstract

In metal powder processing equipment where metal powder is sequentially laminated on a table of a chamber and laser beam melting or electron beam melting is performed or cutting and shaping are performed by a rotating tool subsequent to melting, a first temperature adjusting unit is placed at a lower bottom portion of the table and a second temperature adjusting unit is disposed in contact with and around the outer wall of the chamber and both units are simultaneously heated or cooled; a room partially enclosing a metal powder reserve tank and a metal powder supply pipe is provided with a third temperature adjusting unit, the temperature of which is set to average temperature of the second temperature adjusting unit before the second one actuates, so that deterioration of dimensional precision in processing and deterioration of metal powder quality can be prevented by keeping heating temperature constant.