The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Mar. 28, 2017
Filed:
Feb. 04, 2016
Saudi Arabian Oil Company, Dhahran, SA;
King Fahd University of Petroleum and Minerals, Dhahran, SA;
Musaed Salem Al-Ghrami, Dhahran, SA;
Cemal Ercan, Dhahran, SA;
Sulaiman S. Al-Khattaf, Dhahran, SA;
Mohammed Abdul Bari Siddiqui, Dhahran, SA;
Abdullah M. Aitani, Al-Khobar, SA;
Abstract
Embodiments of the invention provide a method for the fluid catalytic cracking of a heavy hydrocarbon feedstock. According to at least one embodiment, the method includes supplying the heavy hydrocarbon feedstock to a reaction zone having a catalyst, such that both the heavy hydrocarbon feedstock and the catalyst are in contact in a down-flow mode, wherein said contact between the heavy hydrocarbon feedstock and the catalyst takes place in a fluidized catalytic cracking apparatus having a separation zone, a stripping zone, and a regeneration zone. The method further includes maintaining the reaction zone at a temperature of between 500 and 600° C., such that the hydrocarbon feedstock converts into a cracked hydrocarbon effluent comprising light olefins, gasoline, and diesel. The catalyst includes between 10 and 20% by weight of a phosphorous modified sub-micron ZSM-5, between 10 and 20% by weight of an ultra-stable Y-type zeolite, between 20 and 30% by weight of a pseudoboehmite alumina, and between 20 and 40% by weight of kaolin. The phosphorous modified sub-micron ZSM-5 has an average crystal size between 50 and 400 nm, inclusive, and a silica to alumina ratio of 1:2 to 1:4, inclusive.