The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 21, 2017

Filed:

Feb. 06, 2012
Applicants:

Ettore Anelli, Bergamo, IT;

Mariano Armengol, Bergamo, IT;

Paolo Novelli, Bergamo, IT;

Federico Tintori, Bergamo, IT;

Inventors:

Ettore Anelli, Bergamo, IT;

Mariano Armengol, Bergamo, IT;

Paolo Novelli, Bergamo, IT;

Federico Tintori, Bergamo, IT;

Assignee:

DALMINE S.P.A., Bergamo, IT;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 10/00 (2006.01); C21D 8/10 (2006.01); C21D 1/18 (2006.01); C21D 6/00 (2006.01); C21D 9/08 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/08 (2006.01); C22C 38/22 (2006.01); C22C 38/24 (2006.01); C22C 38/00 (2006.01); C22C 38/42 (2006.01); C22C 38/44 (2006.01); C22C 38/46 (2006.01); C22C 38/50 (2006.01); C22C 38/60 (2006.01);
U.S. Cl.
CPC ...
C21D 8/10 (2013.01); C21D 1/18 (2013.01); C21D 6/002 (2013.01); C21D 9/08 (2013.01); C21D 9/085 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/008 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/08 (2013.01); C22C 38/22 (2013.01); C22C 38/24 (2013.01); C22C 38/42 (2013.01); C22C 38/44 (2013.01); C22C 38/46 (2013.01); C22C 38/50 (2013.01); C22C 38/60 (2013.01); C21D 8/105 (2013.01); C21D 2211/002 (2013.01); C21D 2211/008 (2013.01);
Abstract

Low-alloy steels and methods of manufacturing pipes having a wall thickness greater than or equal to about 8 mm and less than or equal to about 35 mm therefrom are provided. In one embodiment, a steel composition is processed that yields an average prior austenite grain size greater than about 15 or 20 μm and smaller than about 100 μm. A quenching sequence has been determined that yields a microstructure of greater than or equal to about 60% martensite by volume, and less than or equal to about 40% by volume lower bainite, without substantial formation of ferrite, upper bainite, or granular bainite. The yield strength of the quenched and tempered pipes may be greater than about 70 ksi, 80 ksi, or 90 ksi. The quenched and tempered pipes are suitable for 70 ksi, 80 ksi, and 90 ksi grades and resistant to sulfide stress corrosion cracking.