The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 28, 2017

Filed:

Apr. 22, 2016
Applicant:

Sumitomo Metal Mining Co., Ltd., Tokyo, JP;

Inventors:

Mitsuru Yamauchi, Ehime, JP;

Kazuomi Ryoshi, Ehime, JP;

Kensaku Mori, Ehime, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/505 (2010.01); H01M 4/525 (2010.01); H01M 4/04 (2006.01); H01M 10/052 (2010.01); H01M 10/0525 (2010.01); C01G 53/00 (2006.01);
U.S. Cl.
CPC ...
H01M 4/505 (2013.01); C01G 53/00 (2013.01); C01G 53/006 (2013.01); C01G 53/40 (2013.01); C01G 53/42 (2013.01); C01G 53/50 (2013.01); H01M 4/0497 (2013.01); H01M 4/525 (2013.01); H01M 10/052 (2013.01); H01M 10/0525 (2013.01); C01P 2002/50 (2013.01); C01P 2004/03 (2013.01); C01P 2004/61 (2013.01); C01P 2006/11 (2013.01); C01P 2006/40 (2013.01); Y02E 60/122 (2013.01); Y02P 70/54 (2015.11);
Abstract

When producing a nickel composite hydroxide that is a precursor to the cathode active material for a non-aqueous electrolyte secondary battery by supplying an aqueous solution that includes at least a nickel salt, a neutralizing agent and a complexing agent into a reaction vessel while stirring and performing a crystallization reaction, a nickel composite hydroxide slurry is obtained while controlling the ratio of the average particle size per volume of secondary particles of nickel composite hydroxide that is generated inside the reaction vessel with respect to the average particle size per volume of secondary particles of nickel composite hydroxide that is finally obtained so as to be 0.2 to 0.6, after which, while keeping the amount of slurry constant and continuously removing only the liquid component, the crystallization reaction is continued until the average particle size per volume of secondary particles of the nickel composite hydroxide becomes 8.0 μm to 50.0 μm.