The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 31, 2017

Filed:

Jul. 20, 2009
Applicants:

Frederic Pialot, Molssat, FR;

Damien Fombelle, Chappes, FR;

Bozena Voge, Coumon D'Auvergne, FR;

Jose Merino Lopez, Riom, FR;

Inventors:

Frederic Pialot, Molssat, FR;

Damien Fombelle, Chappes, FR;

Bozena Voge, Coumon D'Auvergne, FR;

Jose Merino Lopez, Riom, FR;

Assignees:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08J 3/20 (2006.01); C08L 7/00 (2006.01); B29C 73/16 (2006.01); B60C 5/14 (2006.01); B60C 19/12 (2006.01); C08J 3/22 (2006.01); C08J 3/24 (2006.01); C08L 9/00 (2006.01); C08L 21/00 (2006.01); B29L 30/00 (2006.01); C08K 5/31 (2006.01); C08L 45/00 (2006.01); C08L 101/00 (2006.01);
U.S. Cl.
CPC ...
C08L 7/00 (2013.01); B29C 73/163 (2013.01); B60C 5/14 (2013.01); B60C 19/122 (2013.04); C08J 3/226 (2013.01); C08J 3/247 (2013.01); C08L 9/00 (2013.01); C08L 21/00 (2013.01); B29L 2030/00 (2013.01); C08J 2407/00 (2013.01); C08J 2409/00 (2013.01); C08J 2421/00 (2013.01); C08K 5/31 (2013.01); C08L 45/00 (2013.01); C08L 101/00 (2013.01);
Abstract

A process for manufacturing a self-sealing elastomer composition, said process comprising the following steps: a masterbatch, comprising at least one diene elastomer and more than 30 phr of a hydrocarbon resin, is firstly manufactured by compounding these various components in a mixer at a temperature or up to a temperature called the 'hot compounding' temperature which is above the softening point of the hydrocarbon resin; and then at least one crosslinking system is incorporated into the masterbatch thus prepared, by compounding everything in the same mixer or in a different mixer, at a temperature or up to a temperature which is kept below 100° C., in order to obtain said self-sealing composition.