The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 31, 2017

Filed:

Nov. 12, 2012
Applicant:

Evonik Degussa Gmbh, Essen, DE;

Inventors:

Laurent Wattebled, Dusseldorf, DE;

Jorg Harren, Baesweiler, DE;

Matthias Naumann, Hamburg, DE;

Franck Furno, Heiligenhaus, DE;

Matthias Lobert, Essen, DE;

Rainer Teni, Moers, DE;

Assignee:

Evonik Degussa GmbH, Essen, DE;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C08J 3/24 (2006.01); A61L 15/24 (2006.01); A61L 15/22 (2006.01); B01J 20/30 (2006.01); B01J 20/26 (2006.01); C08F 216/14 (2006.01); C08F 220/06 (2006.01); A61L 15/60 (2006.01); C08F 222/10 (2006.01);
U.S. Cl.
CPC ...
A61L 15/225 (2013.01); A61L 15/24 (2013.01); A61L 15/60 (2013.01); B01J 20/267 (2013.01); B01J 20/3064 (2013.01); C08F 220/06 (2013.01); C08J 3/245 (2013.01); C08F 216/1416 (2013.01); C08F 222/1006 (2013.01); C08J 2333/02 (2013.01);
Abstract

This invention relates to a method for producing a water-absorbing polymer, including the following steps: (i) mixing (α1) 0.1 to 99.999 wt % polymerizable, ethylenically unsaturated, acid-group-containing monomers; (α2) 0 to 70 wt % polymerized ethylenically unsaturated, monomers copolymerizable with (α1); (α3) 0.00 1 to 10 wt %, cross-linking agent(s); (α4) 0 to 30 wt % water-soluble polymers; and (α5) 0 to 20 wt % additive(s), wherein the total quantity by weight of (α1) to (α5) amounts to 100 wt %, (ii) radical polymerization while cross-linking, in order to form a hydrogel polymer, (iii) drying the hydrogel polymer, (iv) grinding and sifting the water-absorbing polymer, (v) surface post-cross-linking the hydrogel polymer, and (vi) drying and processing the polymer, wherein, before the admixture of the initiator and the start of radical polymerization, 0.01 to 5 wt % of a surfactant, relative to acrylic acid, 0.01 to 5 wt % foaming agent, are added.