The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 10, 2017

Filed:

Jul. 29, 2011
Applicants:

Masakazu Seki, Chiyoda-ku, JP;

Satoshi Suzuki, Chiyoda-ku, JP;

Kenji Yamamoto, Chuo-ku, JP;

Tomohiko Furutani, Chuo-ku, JP;

Inventors:

Masakazu Seki, Chiyoda-ku, JP;

Satoshi Suzuki, Chiyoda-ku, JP;

Kenji Yamamoto, Chuo-ku, JP;

Tomohiko Furutani, Chuo-ku, JP;

Assignees:

UACJ Corporation, Tokyo, JP;

UACJ Foil Corporation, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/66 (2006.01); B21B 1/40 (2006.01); C22C 1/02 (2006.01); C22C 21/00 (2006.01); C22F 1/04 (2006.01); B22D 11/06 (2006.01); B22D 11/12 (2006.01); B22D 25/04 (2006.01); C22F 1/00 (2006.01); B23K 35/28 (2006.01); B23K 35/02 (2006.01); H01G 11/68 (2013.01); H01M 10/052 (2010.01);
U.S. Cl.
CPC ...
H01M 4/662 (2013.01); B21B 1/40 (2013.01); B22D 11/0622 (2013.01); B22D 11/1206 (2013.01); B22D 25/04 (2013.01); B23K 35/0233 (2013.01); B23K 35/286 (2013.01); C22C 1/026 (2013.01); C22C 21/00 (2013.01); C22F 1/00 (2013.01); C22F 1/04 (2013.01); H01G 11/68 (2013.01); H01M 10/052 (2013.01); Y02E 60/13 (2013.01); Y02T 10/7011 (2013.01); Y02T 10/7022 (2013.01); Y10T 428/12431 (2015.01);
Abstract

An object of the present invention is to provide an aluminum alloy foil for an electrode current collector, the foil having a high strength after the drying step while keeping a high electrical conductivity. Disclosed is a method for manufacturing an aluminum alloy foil for electrode current collector, including: maintaining an aluminum alloy ingot comprising 0.1 to 0.5% of Fe, 0.01 to 0.3% of Si, 0.01 to 0.2% of Cu, 0.01% or less of Mn, with the rest being Al and unavoidable impurities, at 550 to 620° C. for 1 to 20 hours, and subjecting the resulting ingot under a hot rolling with a starting temperature of 500° C. or higher and an end-point temperature of 255 to 300° C.