The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 10, 2017

Filed:

Sep. 12, 2011
Applicants:

Daniel Wasserfallen, Mainz, DE;

Martin Droll, Schlangen, DE;

Oliver Seewald, Marsberg, DE;

Wolfgang Bremser, Paderborn, DE;

Michael Schwamb, Frankfurt, DE;

Cindy Ettrich, Frankfurt am Main, DE;

Vera Sotke, Frankfurt, DE;

Inventors:

Daniel Wasserfallen, Mainz, DE;

Martin Droll, Schlangen, DE;

Oliver Seewald, Marsberg, DE;

Wolfgang Bremser, Paderborn, DE;

Michael Schwamb, Frankfurt, DE;

Cindy Ettrich, Frankfurt am Main, DE;

Vera Sotke, Frankfurt, DE;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B05D 3/00 (2006.01); B05D 7/14 (2006.01); B05D 7/16 (2006.01); B05D 7/00 (2006.01); C09D 5/08 (2006.01); C23C 18/54 (2006.01); C25D 13/00 (2006.01); B05D 1/18 (2006.01);
U.S. Cl.
CPC ...
B05D 3/002 (2013.01); B05D 7/142 (2013.01); B05D 7/16 (2013.01); B05D 7/51 (2013.01); C09D 5/088 (2013.01); C23C 18/54 (2013.01); C25D 13/00 (2013.01); B05D 1/18 (2013.01); B05D 7/54 (2013.01); Y10T 428/24975 (2015.01); Y10T 428/265 (2015.01);
Abstract

A method for electroless coating of a substrate by applying an activating coat of polyelectrolyte or salt with a first aqueous composition, rinsing of the activating coat such that the activating coat is not entirely removed The activated surface that has remained after rinsing is then contacted with an aqueous composition in the form of a solution, emulsion or suspension to form an organic secondary coat (precipitation coat), and drying. The activating coat contains at least one cationic polyelectrolyte or at least one cationic salt in solution in water. The aqueous composition which forms the secondary coat contains constituents which can be precipitated, deposited and/or salted out and which are anionically, zwitterionically, sterically or cationically stabilized. The dry film formed in the process, which is made of the activating coat and the secondary coat, has a thickness of at least 1 μm.