The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 27, 2016

Filed:

Jun. 07, 2013
Applicant:

Tdk Corporation, Tokyo, JP;

Inventor:

Hitoshi Taguchi, Tokyo, JP;

Assignee:

TDK Corporation, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01F 1/36 (2006.01); H01F 1/11 (2006.01); C04B 35/626 (2006.01); C04B 35/26 (2006.01); C01G 49/00 (2006.01); H01F 1/34 (2006.01); H01F 41/02 (2006.01);
U.S. Cl.
CPC ...
H01F 1/36 (2013.01); C01G 49/0027 (2013.01); C01G 49/0036 (2013.01); C04B 35/26 (2013.01); C04B 35/6261 (2013.01); C04B 35/62675 (2013.01); H01F 1/11 (2013.01); H01F 1/344 (2013.01); H01F 41/0266 (2013.01); C01P 2004/03 (2013.01); C01P 2004/51 (2013.01); C01P 2004/62 (2013.01); C01P 2006/12 (2013.01); C01P 2006/42 (2013.01); C04B 2235/3201 (2013.01); C04B 2235/3213 (2013.01); C04B 2235/3427 (2013.01); C04B 2235/442 (2013.01); C04B 2235/549 (2013.01); C04B 2235/5409 (2013.01); C04B 2235/5445 (2013.01); C04B 2235/724 (2013.01); C04B 2235/784 (2013.01); C04B 2235/785 (2013.01); Y10T 428/2982 (2015.01);
Abstract

Provided is a method for producing Sr ferrite particles for sintered magnets, the method includes: a mixing step of mixing an iron compound, a strontium compound, and an alkali metal compound which includes at least one of K and Na as a constituent element and which does not include Cl and S as the constituent element to prepare a mixture; and a calcining step of firing the mixture at 850° C. to 1100° C. to obtain Sr ferrite particles in which an average particle size of primary particles is 0.2 to 1.0 μm. In the mixing step, the alkali metal compound is mixed in such a manner that a total amount of K and Na becomes 0.03 to 1.05% by mass in terms of KO and NaO with respect to a total amount of a powder of the iron compound and a powder of the strontium compound.