The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 20, 2016

Filed:

Aug. 15, 2012
Applicants:

Shinya Teramoto, Tokyo, JP;

Manabu Kubota, Tokyo, JP;

Inventors:

Shinya Teramoto, Tokyo, JP;

Manabu Kubota, Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 38/38 (2006.01); F16F 1/02 (2006.01); C21D 1/06 (2006.01); C21D 6/00 (2006.01); C21D 9/02 (2006.01); C22C 38/00 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/34 (2006.01); C21D 8/06 (2006.01); C22C 38/02 (2006.01); C22C 38/22 (2006.01); C22C 38/24 (2006.01); C22C 38/26 (2006.01); C22C 38/28 (2006.01);
U.S. Cl.
CPC ...
F16F 1/02 (2013.01); C21D 1/06 (2013.01); C21D 6/008 (2013.01); C21D 8/065 (2013.01); C21D 9/02 (2013.01); C22C 38/001 (2013.01); C22C 38/002 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/22 (2013.01); C22C 38/24 (2013.01); C22C 38/26 (2013.01); C22C 38/28 (2013.01); C22C 38/34 (2013.01); C22C 38/38 (2013.01);
Abstract

The present invention provides a spring steel, which is finally formed into a spring, by making use of, at a maximum, the temper softening resistance effect due to alloying elements while suppressing the formation of hard inclusions of SiOand the generation of decarburization, which may cause deterioration of fatigue characteristics of the spring. The spring steel is characterized by comprising, in % by mass, C: 0.50 to 0.70%, Si: 1.00 to 5.00%, Mn: 0.30 to 2.00%, P: 0.0002 to 0.0500%, S: 0.0002 to 0.0500%, Cr: 0.10 to 3.50%, Al: 0.0005 to 0.0500%, and N: 0.0020 to 0.0100%, with the balance being Fe and inevitable impurities, wherein the H-value defined by the following equation (a) is 160 or more, and the C-value defined by the following equation (b) is 3.25 or less:H=33.6[C]+10.0[Si]+5.95[Mn]+11.1[Cr]+90.0  (a),andC=[Si]/[Mn]  (b).