The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 29, 2016

Filed:

May. 28, 2010
Applicants:

Satoru Hommura, Chiyoda-ku, JP;

Susumu Saito, Chiyoda-ku, JP;

Tetsuji Shimohira, Chiyoda-ku, JP;

Atsushi Watakabe, Chiyoda-ku, JP;

Inventors:

Satoru Hommura, Chiyoda-ku, JP;

Susumu Saito, Chiyoda-ku, JP;

Tetsuji Shimohira, Chiyoda-ku, JP;

Atsushi Watakabe, Chiyoda-ku, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01B 1/12 (2006.01); H01M 8/10 (2016.01); C08F 216/14 (2006.01);
U.S. Cl.
CPC ...
H01B 1/122 (2013.01); C08F 216/1408 (2013.01); H01M 8/1023 (2013.01); H01M 8/1039 (2013.01); H01M 8/1081 (2013.01); Y02E 60/521 (2013.01); Y02P 70/56 (2015.11);
Abstract

It is to provide an electrolyte material with which an increase in the water content can be suppressed even when the ion exchange capacity of a polymer having repeating units based on a monomer having a dioxolane ring is high; and a membrane/electrode assembly excellent in the power generation characteristics under low or no humidity conditions and under high humidity conditions. It is to use an electrolyte material, which comprises a polymer (H) having ion exchange groups converted from precursor groups in a polymer (F), and having an ion exchange capacity of at least 1.35 meq/g dry resin, the polymer (F) having repeating units (A) based on a perfluoromonomer having a precursor group of an ion exchange group and a dioxolane ring and repeating units (B) based on a perfluoromonomer having no precursor group and having a dioxolane ring, and having a TQ of at least 200° C., which is a temperature at which the melt volume rate becomes 100 mm/sec when the polymer (F) is subjected to melt-extrusion under an extrusion pressure condition of 2.94 MPa from a nozzle having a length of 1 mm and an inner diameter of 1 mm.