The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 29, 2016

Filed:

Jan. 31, 2013
Applicant:

Hewlett-packard Development Company, L.p., Houston, TX (US);

Inventors:

Bor-Jiunn Niu, San Diego, CA (US);

Haigang Chen, San Diego, CA (US);

Jason Swei, San Diego, CA (US);

Sandeep Bangaru, San Diego, CA (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B41M 5/00 (2006.01); C09D 7/12 (2006.01); B41M 5/52 (2006.01); C09D 129/04 (2006.01); C09D 177/00 (2006.01); C09D 179/02 (2006.01); C08G 73/02 (2006.01); C08L 91/06 (2006.01);
U.S. Cl.
CPC ...
C09D 7/1233 (2013.01); B41M 5/52 (2013.01); B41M 5/5218 (2013.01); B41M 5/5227 (2013.01); B41M 5/5236 (2013.01); B41M 5/5245 (2013.01); B41M 5/5254 (2013.01); B41M 5/5263 (2013.01); C08G 73/0293 (2013.01); C09D 7/1216 (2013.01); C09D 7/1275 (2013.01); C09D 7/1283 (2013.01); C09D 129/04 (2013.01); C09D 177/00 (2013.01); C09D 179/02 (2013.01); B41M 5/0017 (2013.01); B41M 5/5281 (2013.01); C08L 91/06 (2013.01);
Abstract

The present disclosure provides swellable pre-treatment compositions, printable media, and related methods. As such, a swellable pre-treatment coating for a print medium can include an evaporable solvent, a matrix, and a wax. The matrix can include from 10 wt % to 20 wt % of a fixer, from 25 wt % to 35 wt % of aluminum chlorohydrate, from 0.5 wt % to 10 wt % of a first binder, from 20 wt % to 30 wt % of a second cross-linkable binder, and from 1 wt % to 5 wt % of a cross-linker. The wax can be present at from 10 wt % to 20 wt %, The weight percentages of the matrix and the wax are based on a total amount present in the swellable pre-treatment coating after removal of the evaporable solvent.


Find Patent Forward Citations

Loading…