The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 22, 2016

Filed:

Sep. 20, 2013
Applicant:

Panasonic Intellectual Property Management Co., Ltd., Osaka, JP;

Inventors:

Tadayoshi Takahashi, Osaka, JP;

Kanji Kawakami, Osaka, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 2/08 (2006.01); H01M 10/052 (2010.01); H01M 2/04 (2006.01); H01M 2/02 (2006.01);
U.S. Cl.
CPC ...
H01M 2/08 (2013.01); H01M 2/02 (2013.01); H01M 2/0202 (2013.01); H01M 2/0237 (2013.01); H01M 2/0413 (2013.01); H01M 10/052 (2013.01); H01M 2/0222 (2013.01); H01M 2/0465 (2013.01); H01M 2220/20 (2013.01); H01M 2220/30 (2013.01); Y02E 60/122 (2013.01);
Abstract

Provided is a non-aqueous electrolyte battery including: a power-generating element; and a battery container configured to house the power-generating element. The power-generating element includes: a positive electrode; a negative electrode; a separator interposed between the positive and negative electrodes; and a non-aqueous electrolyte. The battery container includes: a battery case having an opening; a sealing plate configured to close the opening; and a gasket interposed between the battery case and the sealing plate. The gasket includes a PFA resin being a copolymer of tetrafluoroethylene and perfluoroalkyl vinyl ether, and at least a part of the PFA resin has undergone a melting treatment 2 to 20 times to be a first component. The melting treatment includes heating the PFA resin to a melting temperature of 310° C. to 450° C. for melting and then cooling the PFA resin back to a solid.