The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 15, 2016

Filed:

Mar. 29, 2012
Applicants:

Huawei Zhang, Shanghai, CN;

Yaping Wu, Shanghai, CN;

Yu Gong, Shanghai, CN;

Yezhong Sun, Shanghai, CN;

Hongxu Hei, Shanghai, CN;

Inventors:

Huawei Zhang, Shanghai, CN;

Yaping Wu, Shanghai, CN;

Yu Gong, Shanghai, CN;

Yezhong Sun, Shanghai, CN;

Hongxu Hei, Shanghai, CN;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C21D 6/00 (2006.01); H01F 1/147 (2006.01); C21D 8/12 (2006.01); C21D 1/26 (2006.01); C22C 38/02 (2006.01); H01F 41/00 (2006.01); C21D 8/02 (2006.01); C21D 8/04 (2006.01); C21D 9/00 (2006.01); C21D 9/70 (2006.01);
U.S. Cl.
CPC ...
H01F 1/14766 (2013.01); C21D 1/26 (2013.01); C21D 6/00 (2013.01); C21D 6/008 (2013.01); C21D 8/021 (2013.01); C21D 8/041 (2013.01); C21D 8/1205 (2013.01); C21D 8/1216 (2013.01); C21D 8/1244 (2013.01); C21D 9/0081 (2013.01); C21D 9/70 (2013.01); C22C 38/02 (2013.01); H01F 41/00 (2013.01); C21D 2201/05 (2013.01);
Abstract

A hot rolled silicon steel producing method comprises: silicon steel slab heating process, rough rolling process and finish rolling process. The heating process comprises a pre-heating stage, a heating stage and a soaking stage. The pre-heating stage satisfies the following formula (1). In the formula, VTp is a temperature increasing rate, in the pre-heating stage, whose unit is ° C./min; t is a total heating time of the slab in the heating furnace, and t=180-240 min; and Tc is an initial temperature when the slab is put into the furnace, whose unit is ° C. By using the foregoing formula, the heating process and the rough rolling process are changed, an occurrence rate of edge defects during the production of the hot rolled silicon steel can be reduced, and the hot rolled silicon steel with good surface quality can be produced.