The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 25, 2016

Filed:

Jan. 28, 2014
Applicant:

Saudi Basic Industries Corporation, Riyadh, SA;

Inventor:

Zahir Bashir, Riyadh, SA;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B29C 43/00 (2006.01); C08J 5/00 (2006.01); C08G 63/00 (2006.01); B29K 67/00 (2006.01);
U.S. Cl.
CPC ...
B29C 43/003 (2013.01); B29C 43/006 (2013.01); B29K 2067/00 (2013.01); B29K 2995/0041 (2013.01);
Abstract

A process for making a shaped part from a polymer selected from polyethylene terephthalate (PET) and polyethylene terephthalate (PET) and polyethylene naphthalate (PEN) by using a compacting tool comprising a die having a cavity and a punch having an outer surface. The process comprises the steps of: a) placing particles of the polymer in the cavity of the die heated to a compaction temperature, wherein the polymer has an intrinsic viscosity of at least 0.45 dL/g wherein the particles are a mixture of first particles with a particle size of 0.5-4000 μm and second particles with a particle size of 1000-4000 μm b) pressing the particles in the die cavity at a pressure of at least 3 MPa for 5-15 minutes while maintaining the temperature of the die at the compaction temperature and c) removing the shaped part from the die cavity. When the polymer is PET, the compaction temperature is 235-259° C. When the polymer is PEN, the compaction temperature is 250-275 ° C.