The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 11, 2016

Filed:

Oct. 03, 2011
Applicants:

Seiichi Katou, Kodaira, JP;

Satoshi Horie, Kodaira, JP;

Inventors:

Seiichi Katou, Kodaira, JP;

Satoshi Horie, Kodaira, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08J 3/20 (2006.01); B60C 1/00 (2006.01); C08K 5/39 (2006.01); B29C 47/60 (2006.01); B29B 7/18 (2006.01); B29B 7/48 (2006.01); B29B 7/88 (2006.01);
U.S. Cl.
CPC ...
C08J 3/20 (2013.01); B29C 47/6056 (2013.01); B60C 1/00 (2013.01); B60C 1/0016 (2013.04); C08K 5/39 (2013.01); B29B 7/183 (2013.01); B29B 7/48 (2013.01); B29B 7/88 (2013.01);
Abstract

The present invention provides a method for producing a rubber composition containing a rubber component (A) of at least one selected from natural rubbers and synthetic dienic rubbers, an inorganic filler (B), a silane coupling agent (C) and an acidic compound (D), wherein the rubber composition is kneaded in multiple stages, and in the final stage of kneading, the acidic compound (D) is added, and the highest temperature of the rubber composition in the final stage of kneading is from 60 to 120° C. The production method enables production of a rubber composition having a low-heat-generation property while successfully preventing the coupling function activity of the silane coupling agent from lowering.