The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 27, 2016

Filed:

Sep. 25, 2013
Applicant:

University of Connecticut, Farmington, CT (US);

Inventors:

Steven L. Suib, Storrs, CT (US);

Altug Suleyman Poyraz, Willington, CT (US);

Assignee:

UNIVERSITY OF CONNECTICUT, Farmington, CT (US);

Attorneys:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C01B 13/32 (2006.01); B01J 21/06 (2006.01); B82Y 30/00 (2011.01); C01G 1/02 (2006.01); C01B 19/00 (2006.01); C01B 33/113 (2006.01); C01B 35/10 (2006.01); C01B 33/12 (2006.01); C01B 37/02 (2006.01); C01G 23/053 (2006.01); C01G 25/02 (2006.01); C01G 45/02 (2006.01); C01G 49/06 (2006.01); C01G 51/04 (2006.01); C01G 3/02 (2006.01);
U.S. Cl.
CPC ...
C01B 13/328 (2013.01); B82Y 30/00 (2013.01); C01B 19/004 (2013.01); C01B 33/113 (2013.01); C01B 33/124 (2013.01); C01B 35/1027 (2013.01); C01B 37/02 (2013.01); C01G 1/02 (2013.01); C01G 3/02 (2013.01); C01G 23/053 (2013.01); C01G 25/02 (2013.01); C01G 45/02 (2013.01); C01G 49/06 (2013.01); C01G 51/04 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2004/04 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); C01P 2006/14 (2013.01); C01P 2006/16 (2013.01); C01P 2006/17 (2013.01);
Abstract

A process for preparing a mesoporous metal oxide, i.e., transition metal oxide, Lanthanide metal oxide, a post-transition metal oxide and metalloid oxide. The process comprises providing a micellar solution comprising a metal precursor, an interface modifier, a hydrotropic ion precursor, and a surfactant; and heating the micellar solution at a temperature and for a period of time sufficient to form the mesoporous metal oxide. A mesoporous metal oxide prepared by the above process. A method of controlling nano-sized wall crystallinity and mesoporosity in mesoporous metal oxides. The method comprises providing a micellar solution comprising a metal precursor, an interface modifier, a hydrotropic ion precursor, and a surfactant; and heating the micellar solution at a temperature and for a period of time sufficient to control nano-sized wall crystallinity and mesoporosity in the mesoporous metal oxides. Mesoporous metal oxides and a method of tuning structural properties of mesoporous metal oxides.