The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 27, 2016

Filed:

Oct. 20, 2014
Applicant:

United Technologies Corporation, Hartford, CT (US);

Inventors:

Lea Kennard Castle, Vernon, CT (US);

Mario P. Bochiechio, Vernon, CT (US);

Assignee:

United Technologies Corporation, Farmington, CT (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B22D 17/14 (2006.01); B22D 17/20 (2006.01); B22D 17/22 (2006.01); B22D 30/00 (2006.01); B22D 17/02 (2006.01); B22D 21/00 (2006.01); B22D 21/02 (2006.01); B22C 9/06 (2006.01); B22C 9/08 (2006.01); C22C 19/03 (2006.01);
U.S. Cl.
CPC ...
B22D 17/02 (2013.01); B22C 9/067 (2013.01); B22C 9/088 (2013.01); B22D 17/14 (2013.01); B22D 17/145 (2013.01); B22D 17/20 (2013.01); B22D 17/22 (2013.01); B22D 21/005 (2013.01); B22D 21/025 (2013.01); B22D 30/00 (2013.01); B22D 17/2218 (2013.01); C22C 19/03 (2013.01); Y10T 428/12389 (2015.01);
Abstract

A die casting and a method for die casting a metal having a melting temperature of at least 1500° F. (815° C.) are disclosed. A molten volume of metal is injected to a casting die which includes a main cavity corresponding to an as-cast structure, a first reservoir, and a first runner arrangement. The first runner arrangement is configured to fluidly communicate molten metal between the first reservoir and the main cavity. After the injecting step, the casting die is sealed. The injected molten volume of metal is equiaxially solidified generally from a first portion of the main cavity distal to the first reservoir toward a second portion of the main cavity proximal to the first reservoir. During the equiaxial solidifying step, the main cavity is backfilled with at least a portion of the injected molten volume via the first runner arrangement.