The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 20, 2016

Filed:

Mar. 28, 2006
Applicants:

Kei Yonezawa, Tokyo, JP;

Takashi Sato, Fukushima, JP;

Tsuyoshi Okawa, Fukushima, JP;

Yoshikatsu Yamamoto, Fukushima, JP;

Inventors:

Kei Yonezawa, Tokyo, JP;

Takashi Sato, Fukushima, JP;

Tsuyoshi Okawa, Fukushima, JP;

Yoshikatsu Yamamoto, Fukushima, JP;

Assignee:

Sony Corporation, Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01M 4/13 (2010.01); H01M 4/525 (2010.01); H01M 4/38 (2006.01); H01M 10/04 (2006.01); H01M 10/0525 (2010.01); H01M 10/0569 (2010.01); H01M 10/0587 (2010.01); H01M 10/42 (2006.01); H01M 4/131 (2010.01); H01M 4/133 (2010.01); H01M 4/485 (2010.01); H01M 4/505 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/525 (2013.01); H01M 4/38 (2013.01); H01M 10/0436 (2013.01); H01M 10/0525 (2013.01); H01M 10/0569 (2013.01); H01M 10/0587 (2013.01); H01M 10/4235 (2013.01); H01M 4/131 (2013.01); H01M 4/133 (2013.01); H01M 4/485 (2013.01); H01M 4/505 (2013.01); H01M 2004/028 (2013.01); H01M 2010/4292 (2013.01); H01M 2300/0037 (2013.01); Y02E 60/122 (2013.01);
Abstract

A battery capable of improving load characteristics, low-temperature characteristics and high-temperature cycle characteristics is provided. A cathode () includes a lithium cobalt complex oxide represented by LiCoMIMIIO(MI includes at least one kind selected from the group consisting of Al, Cr, V, Mn and Fe, MII includes at least one kind selected from the group consisting of Mg and Ca, 0.9≦a≦1.1, 0.9≦x<1, 0.001≦y≦0.05, 0.001≦z≦0.05, x+y+z=1), and further includes Zr as a sub-component element. The content of Zr is within a range from 0.01 mol % to 10 mol % both inclusive as a ratio (Zr/Co) of Zr to Co in the lithium cobalt complex oxide.