The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 06, 2016

Filed:

Aug. 08, 2013
Applicant:

Ut-battelle, Llc, Oak Ridge, TN (US);

Inventors:

David E. Holcomb, Oak Ridge, TN (US);

Govindarajan Muralidharan, Knoxville, TN (US);

Dane F. Wilson, Oak Ridge, TN (US);

Assignee:

UT-Battelle, LLC, Oak Ridge, TN (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 19/05 (2006.01); C22C 19/00 (2006.01); C22F 1/10 (2006.01);
U.S. Cl.
CPC ...
C22C 19/057 (2013.01); C22C 19/007 (2013.01); C22F 1/10 (2013.01);
Abstract

An essentially Fe- and Co-free alloy is composed essentially of, in terms of weight percent: 6.0 to 7.5 Cr, 0 to 0.15 Al, 0.5 to 0.85 Mn, 11 to 19.5 Mo, 0.03 to 4.5 Ta, 0.01 to 9 W, 0.03 to 0.08 C, 0 to 1 Re, 0 to 1 Ru, 0 to 0.001 B, 0.0005 to 0.005 N, balance Ni, the alloy being characterized by, at 850° C., a yield strength of at least 25 Ksi, a tensile strength of at least 38 Ksi, a creep rupture life at 12 Ksi of at least 25 hours, and a corrosion rate, expressed in weight loss [g/(cmsec)]10during a 1000 hour immersion in liquid FLiNaK at 850° C., in the range of 3 to 10.