The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 30, 2016

Filed:

Jul. 14, 2006
Applicants:

Shintaro Kikuchi, Saitama, JP;

Kotaro Takita, Nasushiobara, JP;

Koichi Kono, Asaka, JP;

Inventors:

Shintaro Kikuchi, Saitama, JP;

Kotaro Takita, Nasushiobara, JP;

Koichi Kono, Asaka, JP;

Assignee:

TORAY BATTERY SEPARATOR FILM CO., LTD., Nasushibara-shi, Tochigi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 2/16 (2006.01); B01D 67/00 (2006.01); B01D 69/02 (2006.01); B01D 69/12 (2006.01); B01D 71/26 (2006.01); B29C 55/02 (2006.01); B29C 55/16 (2006.01); B32B 27/32 (2006.01); B29K 23/00 (2006.01); B29K 105/04 (2006.01); H01M 10/0525 (2010.01); H01M 10/42 (2006.01);
U.S. Cl.
CPC ...
H01M 2/1653 (2013.01); B01D 67/0027 (2013.01); B01D 69/02 (2013.01); B01D 69/12 (2013.01); B01D 71/26 (2013.01); B29C 55/023 (2013.01); B29C 55/16 (2013.01); B32B 27/32 (2013.01); H01M 2/1686 (2013.01); B01D 2325/22 (2013.01); B01D 2325/24 (2013.01); B29K 2023/065 (2013.01); B29K 2023/0683 (2013.01); B29K 2105/04 (2013.01); H01M 10/0525 (2013.01); H01M 10/4235 (2013.01);
Abstract

A multi-layer, microporous polyolefin membrane having at least three layers, which comprises first microporous layers made of a polyethylene resin for constituting at least both surface layers, and at least one second microporous layer comprising a polyethylene resin and polypropylene and disposed between both surface layers, the heat of fusion (ΔH) of the polypropylene measured by differential scanning calorimetry being 90 J/g or more, and the polypropylene content in the second microporous layer being 50% or less by mass based on 100% by mass of the total of the polyethylene resin and the polypropylene.