The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 02, 2016

Filed:

Aug. 20, 2012
Applicants:

Takayuki Kimura, Tokyo, JP;

Takefumi Okumura, Tokyo, JP;

Hiroo Nishiyama, Tokyo, JP;

Inventors:

Takayuki Kimura, Tokyo, JP;

Takefumi Okumura, Tokyo, JP;

Hiroo Nishiyama, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/36 (2006.01); H01M 4/131 (2010.01); H01M 4/505 (2010.01); H01M 4/525 (2010.01); H01M 10/0587 (2010.01); H01M 10/04 (2006.01); H01M 10/0525 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/364 (2013.01); H01M 4/131 (2013.01); H01M 4/505 (2013.01); H01M 4/525 (2013.01); H01M 10/0431 (2013.01); H01M 10/0525 (2013.01); H01M 10/0587 (2013.01); H01M 2004/028 (2013.01); Y02E 60/122 (2013.01);
Abstract

A high-input and high-output battery having a large capacity while guaranteeing safety is provided. In a lithium ion battery having an electrode wound group in which a positive electrode, a negative electrode, and a separator are wound and an electrolytic solution provided in a battery container, a discharge capacity of the battery being 30 Ah or more, the positive electrode has a current collector and a positive electrode composite applied to both surfaces of the current collector, and the positive electrode composite has following configuration. The positive electrode composite contains a mixed active material of layered lithium nickel manganese cobalt composite oxide (NMC) and spinel lithium manganese oxide (sp-Mn), a density of the positive electrode composite is 2.4 g/cmor more and 2.7 g/cmor less, and a porosity of the active electrode composite is 29.5% or more and 40.0% or less. Furthermore, a weight ratio (NMC/sp-Mn) of the mixed active materials is set to 10/90 or more and 60/40 or less.