The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.
The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.
Patent No.:
Date of Patent:
Aug. 02, 2016
Filed:
Dec. 14, 2011
Yongqiang LU, Shanghai, CN;
Chunguo LV, Shanghai, CN;
Zhicheng Wang, Shanghai, CN;
Bin Chen, Shanghai, CN;
Xiao Chen, Shanghai, CN;
Shishu Xie, Shanghai, CN;
Yongqiang Lu, Shanghai, CN;
Chunguo Lv, Shanghai, CN;
Zhicheng Wang, Shanghai, CN;
Bin Chen, Shanghai, CN;
Xiao Chen, Shanghai, CN;
Shishu Xie, Shanghai, CN;
BAOSHAN IRON & STEEL CO., LTD, Shanghai, CN;
Abstract
A method of producing an extremely thick insulation coating on a surface of an electrical steel, comprises the following steps: 1) preparing a coating liquid—stirring sufficiently the coating liquid for 0.1˜4 hours, with the viscosity of the coating liquid being within 10˜80 S; 2) coating a strip steel—using a double-roller or a tri-roller coating machine, wherein the film thickness and evenness can be controlled by adjusting different parameters; 3) baking the coating—using three sections, that is, a drying section, a baking section and a cooling section, to bake the coating, wherein the temperature in the drying section is 100˜400° C., the temperature in the baking section is 200˜370° C.; the time in the whole drying and solidification section is 33˜144 seconds, wherein the time in the drying section is 9˜39 seconds, and the baking time is 24˜105 seconds; wherein in the baking process, the strip steel having been coated is conveyed in a non-contact way, in particular, the strip steel is conveyed by blowing pressure-adjustable air onto the lower surface to make it float; the air pressure is 0˜2000 Pa; the wet film is kept out of contact with the furnace rollers before it is solidified, guaranteeing that the surface of wet film is intact; 4) online detecting the film thickness.