The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 19, 2016

Filed:

Mar. 29, 2012
Applicants:

Ikuka Hashimoto, Itoigawa, JP;

Hiroyuki Yashima, Itoigawa, JP;

Takeo Mori, Itoigawa, JP;

Inventors:

Ikuka Hashimoto, Itoigawa, JP;

Hiroyuki Yashima, Itoigawa, JP;

Takeo Mori, Itoigawa, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08L 11/00 (2006.01); C09D 111/02 (2006.01); C08F 236/18 (2006.01); C08K 3/22 (2006.01); C08J 5/02 (2006.01); A61B 17/00 (2006.01);
U.S. Cl.
CPC ...
C09D 111/02 (2013.01); C08F 236/18 (2013.01); C08J 5/02 (2013.01); C08K 3/22 (2013.01); A61B 2017/00526 (2013.01); C08J 2311/02 (2013.01);
Abstract

Provided is a polychloroprene latex that shows favorable low-temperature stability without deterioration in the rubber agglutinating property during production of the dip-molded article, a rubber composition, and a dip-molded article, prepared by using the same. Prepared is a polychloroprene latex of a chloroprene copolymer obtained by polymerization of raw monomers at least containing chloroprene and 2,3-dichloro-1,3-butadiene, which is dispersed in water, wherein the 2,3-dichloro-1,3-butadiene content in the raw monomers is controlled to 1 to 30 mass % and the potassium ion content is adjusted to 0.7 to 1.5 parts by mass and the sodium ion content to 0.2 part or less by mass with respect to 100 parts by mass of the solid matter. In addition, a metal oxide: 1 to 10 parts by mass, sulfur: 0.1 to 3 parts by mass, an aging inhibitor: 0.1 to 5 parts by mass and a surfactant: 0.1 to 10 parts by mass, respectively with respect to 100 parts by mass of the solid matter, were added to the chloroprene latex, to give a rubber composition.