The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 12, 2016

Filed:

Apr. 19, 2012
Applicants:

Nobuyuki Akutagawa, Kanagawa, JP;

Hiroyuki Yoneyama, Kanagawa, JP;

Daiki Wakizaka, Kanagawa, JP;

Inventors:

Nobuyuki Akutagawa, Kanagawa, JP;

Hiroyuki Yoneyama, Kanagawa, JP;

Daiki Wakizaka, Kanagawa, JP;

Assignee:
Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
G02B 1/111 (2015.01); B05D 5/06 (2006.01); B05D 3/10 (2006.01); B05D 5/00 (2006.01); B32B 7/02 (2006.01); C08L 27/12 (2006.01); C08K 9/06 (2006.01); C08K 9/04 (2006.01);
U.S. Cl.
CPC ...
G02B 1/111 (2013.01); B05D 3/108 (2013.01); B05D 5/00 (2013.01); B05D 5/063 (2013.01); B32B 7/02 (2013.01); C08K 9/04 (2013.01); C08K 9/06 (2013.01); C08L 27/12 (2013.01); Y10T 428/24975 (2015.01); Y10T 428/3154 (2015.04);
Abstract

The method for producing an antireflection film is provided. The method includes, a step of coating a coating composition including the following components (A) to (D) on a base material to form a coating film, a step of volatilizing the solvent from the coating film for drying the coating film, and a step of curing the coating film to form a cured layer, in which a multilayer structure having different refractive indices from the coating composition is formed: (A) a fluorine-containing polymer with a specific structure, having a polyalkylene oxide group in the molecule, (B) non-surface-modified inorganic fine particles, or inorganic fine particles that are surface-treated with a silane coupling agent having a molecular weight of 600 or less, (C) a curable binder having no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.