The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jun. 14, 2016

Filed:

Nov. 07, 2013
Applicant:

Saudi Basic Industries Corporation, Riyadh, SA;

Inventors:

James W. Kauffman, Katy, TX (US);

Patricia A. Hooks, Houston, TX (US);

Balamurali Krishna R. Nair, Sugar Land, TX (US);

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B01J 23/60 (2006.01); B01J 23/63 (2006.01); B01J 23/78 (2006.01); B01J 23/80 (2006.01); B01J 23/83 (2006.01); B01J 21/04 (2006.01); C07C 5/32 (2006.01); B01J 27/185 (2006.01); B01J 37/08 (2006.01); B01J 37/10 (2006.01); B01J 23/58 (2006.01); B01J 23/62 (2006.01); B01J 27/10 (2006.01); B01J 35/10 (2006.01); B01J 37/00 (2006.01); C07C 5/333 (2006.01);
U.S. Cl.
CPC ...
B01J 21/04 (2013.01); B01J 23/58 (2013.01); B01J 23/62 (2013.01); B01J 27/10 (2013.01); B01J 27/1856 (2013.01); B01J 35/1014 (2013.01); B01J 35/1019 (2013.01); B01J 35/1038 (2013.01); B01J 35/1042 (2013.01); B01J 35/1061 (2013.01); B01J 35/1066 (2013.01); B01J 35/1071 (2013.01); B01J 35/1076 (2013.01); B01J 37/0009 (2013.01); B01J 37/08 (2013.01); B01J 37/10 (2013.01); C07C 5/322 (2013.01); C07C 5/3337 (2013.01); C07C 2521/04 (2013.01); C07C 2523/02 (2013.01); C07C 2523/14 (2013.01); C07C 2523/42 (2013.01); C07C 2523/755 (2013.01); C07C 2523/89 (2013.01); C07C 2527/10 (2013.01); C07C 2527/14 (2013.01);
Abstract

A method of forming a dehydrogenation catalyst support is carried out by forming a mixture comprising a bayerite aluminum hydroxide (Al(OH)) and water into a support material. The support material is particulized. The particulized support material is compressed to a pressure of at least 5,000 psig to form a shaped body. The shaped body is calcined in pure steam at a temperature of at least 750° C. for at least 0.25 hours to form a catalyst support having an average pore diameter of 200 Å or greater. The catalyst support can then be treated with a dehydrogenation catalyst component so that the catalyst support contains the dehydrogenation catalyst component to form a dehydrogenation catalyst that can then be used by contacting a hydrocarbon feed with the catalyst within a reactor in the presence of steam under dehydrogenation reaction conditions suitable to form dehydrogenated hydrocarbon products.