The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 24, 2016

Filed:

Nov. 25, 2008
Applicants:

Nikolai Arjakine, Berlin, DE;

Georg Bostanjoglo, Berlin, DE;

Bernd Burbaum, Übach-Palenberg, DE;

Andres Gasser, Aachen, DE;

Torsten Jambor, Köln, DE;

Stefanie Linnenbrink, Kreuzau, DE;

Torsten Melzer-jokisch, Neuenhagen bei Berlin, DE;

Michael Ott, Mülheim an der Ruhr, DE;

Norbert Pirch, Aachen, DE;

Rolf Wilkenhöner, Kleinmachnow, DE;

Inventors:

Nikolai Arjakine, Berlin, DE;

Georg Bostanjoglo, Berlin, DE;

Bernd Burbaum, Übach-Palenberg, DE;

Andres Gasser, Aachen, DE;

Torsten Jambor, Köln, DE;

Stefanie Linnenbrink, Kreuzau, DE;

Torsten Melzer-Jokisch, Neuenhagen bei Berlin, DE;

Michael Ott, Mülheim an der Ruhr, DE;

Norbert Pirch, Aachen, DE;

Rolf Wilkenhöner, Kleinmachnow, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B23K 26/00 (2014.01); F01D 5/00 (2006.01); B23K 35/00 (2006.01); B23K 26/32 (2014.01);
U.S. Cl.
CPC ...
F01D 5/005 (2013.01); B23K 26/144 (2015.10); B23K 26/32 (2013.01); B23K 26/342 (2015.10); B23K 35/007 (2013.01); B23K 2201/001 (2013.01); B23K 2203/08 (2013.01); F05D 2230/232 (2013.01); F05D 2230/31 (2013.01); F05D 2230/80 (2013.01); Y02T 50/67 (2013.01); Y02T 50/671 (2013.01);
Abstract

A method of welding workpieces of high-temperature superalloys is provided. Welding filler is applied in a plurality of layers to a surface of the workpiece via a heat input zone and a supply zone for supplying the welding filler into the heat input zone. The heat input zone and the supply zone on the one hand and the workpiece surface on the other hand are moved in relation to one another. A polycrystalline weld seam is generated by remelting a previously applied layer of the plurality of layers. Welding parameters are chosen such that a cooling rate during a solidifying of the material is at least 8000 Kelvins per second. Further, a welding apparatus for carrying out such a method is provided.