The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
May. 17, 2016

Filed:

Sep. 18, 2012
Applicant:

Mitsubishi Plastics, Inc., Chiyoda-ku, JP;

Inventors:

Hiroto Yamada, Nagahama, JP;

Tomoyuki Nemoto, Nagahama, JP;

Assignee:

MITSUBISHI PLASTICS, INC., Chiyoda-ku, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B05D 3/02 (2006.01); H01M 2/14 (2006.01); B32B 27/32 (2006.01); H01M 2/16 (2006.01); H01M 10/42 (2006.01); B29C 47/00 (2006.01); B32B 27/08 (2006.01); C09D 1/00 (2006.01); H01M 10/052 (2010.01);
U.S. Cl.
CPC ...
H01M 2/145 (2013.01); B29C 47/00 (2013.01); B32B 27/08 (2013.01); B32B 27/32 (2013.01); C09D 1/00 (2013.01); H01M 2/1646 (2013.01); H01M 2/1653 (2013.01); H01M 2/1686 (2013.01); H01M 10/4235 (2013.01); B32B 2250/24 (2013.01); B32B 2255/10 (2013.01); B32B 2255/26 (2013.01); B32B 2307/518 (2013.01); B32B 2307/704 (2013.01); B32B 2307/724 (2013.01); B32B 2457/10 (2013.01); H01M 10/052 (2013.01); H01M 2220/30 (2013.01);
Abstract

The present invention produces a laminated porous film which improves the stability of an aqueous dispersion of a metal oxide without lowering battery characteristics, while having high binding properties and excellent heat resistance. This laminated porous film exhibits excellent characteristics when used as a separator for batteries. This laminated porous film is produced by forming a porous coating layer on at least one outer surface of a resin porous film, which is formed of a single layer or a laminate of a plurality of layers, by applying a coating liquid that contains a metal oxide, a resin binder and a volatile acid thereto and drying the applied coating liquid. The coating liquid is prepared so that the difference between the pH (pH) of the coating liquid and the pH (pH) of the coating layer is not less than 2.


Find Patent Forward Citations