The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Mar. 01, 2016

Filed:

Dec. 02, 2014
Applicant:

Sanyo Chemical Industries, Ltd., Kyoto-shi, Kyoto, JP;

Inventors:

Yasuhiro Tsudo, Kyoto, JP;

Masaki Inaba, Kyoto, JP;

Koichi Saito, Kyoto, JP;

Hideaki Saito, Kyoto, JP;

Takanori Yamamoto, Kyoto, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08J 3/20 (2006.01); B29C 41/18 (2006.01); C08G 18/73 (2006.01); C08G 18/10 (2006.01); C08G 18/12 (2006.01); C08G 18/42 (2006.01); C08J 3/12 (2006.01); B29K 75/00 (2006.01);
U.S. Cl.
CPC ...
C08J 3/203 (2013.01); B29C 41/18 (2013.01); C08G 18/10 (2013.01); C08G 18/12 (2013.01); C08G 18/42 (2013.01); C08G 18/73 (2013.01); C08J 3/12 (2013.01); C08J 3/20 (2013.01); B29K 2075/00 (2013.01); C08J 2375/00 (2013.01); C08J 2375/04 (2013.01);
Abstract

The present invention is urethane resin particles (C) for slush mold which contain a urethane resin (D) and an additive (N), wherein the particles have a shape factor SF1 of 101 to 200, a shape factor SF2 of 120 to 240, and a central particle diameter of 20 to 500 μm. It is preferred that the urethane resin (D) has a concentration of urea groups of 0.5 to 10% by weight, a total of the concentration of urethane groups and that of the urea groups of 4 to 20% by weight, a melting point of 160 to 260° C. and a glass transition temperature of −65 to 0° C.


Find Patent Forward Citations