The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 23, 2016

Filed:

Sep. 30, 2011
Applicants:

Siong Hui Khoo, Kuantan, MY;

Lawrence Siau Tian Lim, Klang, MY;

Seek Ping Lee, Petaling Jaya, MY;

Eng Long Ong, Petaling Jaya, MY;

Norihide Enomoto, Tokyo, JP;

Inventors:

Siong Hui Khoo, Kuantan, MY;

Lawrence Siau Tian Lim, Klang, MY;

Seek Ping Lee, Petaling Jaya, MY;

Eng Long Ong, Petaling Jaya, MY;

Norihide Enomoto, Tokyo, JP;

Assignees:

KOSSAN SDN BHD, Klang, MY;

MIDORI ANZEN CO., LTD, Tokyo, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
A41D 19/00 (2006.01); C08L 9/02 (2006.01); C08L 9/00 (2006.01); C08K 3/22 (2006.01); C08K 5/095 (2006.01);
U.S. Cl.
CPC ...
C08L 9/02 (2013.01); A41D 19/0055 (2013.01); C08K 3/22 (2013.01); C08L 9/00 (2013.01); C08K 5/095 (2013.01);
Abstract

An elastomer composition comprising, an emulsion which comprises 25-30 weight % of acrylonitrile, 62-71 weight % of butadiene and 4-8 weight % of unsaturated carboxylic acid (total 100 weight %), wherein crosslink is formed by a bond through at least a part of substituent which is possessed by said unsaturated carboxylic acid, and residual substituent of at least one part of substituent which is possessed by said unsaturated carboxylic acid is left in state of free, further Mooney viscosity (ML(100° C.)) of the crosslinked product is 100-220, wherein thin film gloves composed of said elastomer does not contain sulfur which is a crosslinking agent and sulfur composition which is a vulcanization accelerator, thickness is 0.05-0.15 mm, gloves swelling ratio at gloves formation is 240-320, tensile stress is 22-35 MPa, elongation to break is 480-620% and tensile stress at 500% elongation is 15-35 MPa.