The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Feb. 16, 2016

Filed:

Oct. 06, 2011
Applicants:

Sandrine Prat, Mariol, FR;

Jean-marie George, Vendat, FR;

Gilles Barthet, Cusset, FR;

Inventors:

Sandrine Prat, Mariol, FR;

Jean-Marie George, Vendat, FR;

Gilles Barthet, Cusset, FR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01B 19/00 (2006.01); C04B 28/06 (2006.01); C04B 37/02 (2006.01); C04B 40/00 (2006.01); H01B 3/14 (2006.01); H01B 19/04 (2006.01); H01B 17/56 (2006.01); H02G 7/05 (2006.01); C04B 103/32 (2006.01); C04B 111/92 (2006.01);
U.S. Cl.
CPC ...
H01B 19/00 (2013.01); C04B 28/06 (2013.01); C04B 37/026 (2013.01); C04B 40/0067 (2013.01); H01B 3/14 (2013.01); H01B 17/56 (2013.01); H01B 19/04 (2013.01); H02G 7/05 (2013.01); C04B 2103/32 (2013.01); C04B 2111/92 (2013.01); C04B 2237/34 (2013.01); C04B 2237/40 (2013.01); Y10T 29/49227 (2015.01);
Abstract

A method of manufacturing a high-voltage electrical insulator (), having at least one metal insulator element () cemented to a dielectric insulator element () by a cement mortar (), includes at least one of the following steps: preparing the cement mortar () from aluminous cement and sand that are mixed with at least water; assembling the dielectric element () with the metal element (), the mortar () being placed between the dielectric insulator element () and the metal element (); and vibrating the dielectric element () and the metal element () as assembled together, so as to distribute the mortar () between the dielectric element and the metal element (). In order to prepare the mortar (), an active ingredient of the polymer superplasticizer type based on polyglycol methacrylic acid ester is added, and the vibrating is performed for a duration lying in the range 2 seconds to 20 seconds, and preferably in the range 4 seconds to 15 seconds.