The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jan. 05, 2016

Filed:

Nov. 20, 2014
Applicant:

Haimen Senda Decoration Material Co., Ltd, Nantong, CN;

Inventors:

Lixin Huang, Nantong, CN;

Liang Hong, Nantong, CN;

Zhihong Sang, Nantong, CN;

Gang Chen, Nantong, CN;

Hui Jiang, Nantong, CN;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B05D 5/08 (2006.01); C09D 133/08 (2006.01); B05D 5/06 (2006.01); B05D 7/16 (2006.01); B05D 1/02 (2006.01); B08B 17/06 (2006.01); B05D 3/00 (2006.01); B05D 3/02 (2006.01); B44C 1/00 (2006.01);
U.S. Cl.
CPC ...
B05D 5/08 (2013.01); B05D 5/06 (2013.01); B05D 7/16 (2013.01); C09D 133/08 (2013.01); B05D 1/02 (2013.01); B05D 3/002 (2013.01); B05D 3/0272 (2013.01); B05D 2202/15 (2013.01); B08B 17/06 (2013.01); B44C 1/00 (2013.01);
Abstract

The present invention provides a method for preparing a matte anti-fingerprint stainless steel decorative plate. The method comprises the steps of: 1) selecting a polymer coating material, wherein the polymer coating material is formed by mixing a film forming material, an inorganic nano-filler, a solvent and an auxiliary agent, wherein the film forming material comprises the following ingredients based on the weight ratio: 30-50 parts of acrylate composite resin, 5-20 parts of amino resin, and 5-15 parts of epoxy resin; and 1-8 parts of a matting agent and 1-8 parts of an anti-settling agent are added; and 2) performing a spray coating using the polymer coating material, wherein a coating film has a thickness of 1.5-2.5 μm, the precision of the atomization air pressure of a spray gun is controlled at ±0.1 bar during spray coating, and the coating is dried to obtain a finished product and then a matte anti-fingerprint stainless steel decorative plate which has a high-standard matte and anti-fingerprint index is prepared.