The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 08, 2015

Filed:

Feb. 26, 2013
Applicant:

Mitsubishi Plastics, Inc., Chuo-ku, JP;

Inventors:

Takashi Hiruma, Shiga, JP;

Takeyoshi Yamada, Shiga, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
B32B 1/02 (2006.01); C08L 67/04 (2006.01); C08J 5/18 (2006.01); C08L 23/08 (2006.01); C08L 23/10 (2006.01); C08L 23/06 (2006.01); C08L 23/12 (2006.01); C08L 33/06 (2006.01); C08L 53/00 (2006.01);
U.S. Cl.
CPC ...
C08L 67/04 (2013.01); C08J 5/18 (2013.01); C08L 23/0815 (2013.01); C08L 23/10 (2013.01); C08J 2367/04 (2013.01); C08J 2423/04 (2013.01); C08J 2423/08 (2013.01); C08J 2423/10 (2013.01); C08J 2423/14 (2013.01); C08J 2433/06 (2013.01); C08J 2453/00 (2013.01); C08L 23/06 (2013.01); C08L 23/12 (2013.01); C08L 33/06 (2013.01); C08L 53/00 (2013.01); Y10T 428/1328 (2015.01); Y10T 428/1331 (2015.01); Y10T 428/1352 (2015.01); Y10T 428/31797 (2015.04);
Abstract

A heat-shrinkable film having a layer made of a mixed resin containing a polylactic acid resin and a polyolefin resin as the main components, wherein the mass ratio of the polylactic acid resin and the polyolefin resin is 95/5 to 50/50, the polylactic acid resin is a copolymer of D-lactic acid and L-lactic acid or a mixed resin of the copolymer, the D/L ratio of D-lactic acid and L-lactic acid is 3/97 to 15/85 or 85/15 to 97/3, the storage elastic modulus of the polyolefin resin or the soft acrylic resin at 20° C. is ≦100 MPa as measured at an oscillation frequency of 10 Hz and a strain of 0.1%, the film is stretched in at least one direction, and the heat shrinkage ratio of the film in the main shrinking direction is ≧20% as measured after the film is immersed in 80° C. water for 10 seconds.


Find Patent Forward Citations