The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Dec. 01, 2015

Filed:

Jan. 23, 2013
Applicants:

Korea Atomic Energy Research Institute, Daejeon, KR;

Korea Hydro and Nuclear Power Co., Ltd., Gyeongsangbuk-do, KR;

Inventors:

Jeong-Yong Park, Daejeon, KR;

Byoung-Kwon Choi, Daejeon, KR;

Hyun Gil Kim, Daejeon, KR;

Sang Yoon Park, Daejeon, KR;

Yang-Il Jung, Daejeon, KR;

Dong Jun Park, Daejeon, KR;

Yang-Hyun Koo, Daejeon, KR;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C22C 16/00 (2006.01); G21C 3/07 (2006.01); G21C 21/10 (2006.01); C22F 1/18 (2006.01);
U.S. Cl.
CPC ...
G21C 3/07 (2013.01); C22C 16/00 (2013.01); C22F 1/186 (2013.01); G21C 21/10 (2013.01); Y02E 30/40 (2013.01);
Abstract

Disclosed are a zirconium alloy for a nuclear fuel cladding having a good corrosion resistance by reducing an amount of alloying elements and a method of preparing a zirconium alloy nuclear fuel cladding using thereof. The zirconium alloy includes 0.2 to 0.5 wt % of niobium (Nb); 0.2 to 0.6 wt % of iron (Fe); 0.3 to 0.5 wt % of chromium (Cr); 0.1 to 0.15 wt % of oxygen (O); 0.008 to 0.012 wt % of silicon (Si) and a remaining amount of zirconium (Zr). The total amount of the niobium, the iron and the chromium is 1.1 to 1.2 wt %. A good oxidation resistance of the nuclear fuel cladding may be confirmed under accident conditions as well as normal operating conditions of a reactor, thereby improving economic feasibility and safety.