The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 24, 2015

Filed:

Sep. 15, 2010
Applicants:

Tatsuo Tomomori, Yamaguchi, JP;

Koh Yoshioka, Yamaguchi, JP;

Hideyuki Minagi, Yamaguchi, JP;

Inventors:

Tatsuo Tomomori, Yamaguchi, JP;

Koh Yoshioka, Yamaguchi, JP;

Hideyuki Minagi, Yamaguchi, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
F16L 9/14 (2006.01); F16L 58/08 (2006.01); B60K 15/04 (2006.01); C25D 5/36 (2006.01); C25D 3/12 (2006.01); C25D 5/02 (2006.01); B60K 15/03 (2006.01);
U.S. Cl.
CPC ...
F16L 58/08 (2013.01); B60K 15/04 (2013.01); C25D 3/12 (2013.01); C25D 5/02 (2013.01); C25D 5/36 (2013.01); B60K 2015/03486 (2013.01); B60K 2015/047 (2013.01); Y10T 428/12944 (2015.01);
Abstract

A nickel-plated steel sheet for manufacturing a pipe having corrosion resistance against fuel vapor; and a pipe and a fuel supply pipe. In the pipe and fuel supply pipe, a nickel plating layer having a plating thickness of 0.5 to 10 μm is formed on an inner surface of a pipe formed of a steel sheet thus having corrosion resistance against fuel vapor. In the fuel supply pipe formed of a steel sheet for supplying fuel to a fuel tank, the fuel supply pipe includes: a large-diameter pipe portion through which the fuel passes; and a small-diameter pipe portion which makes an upper portion of the large-diameter pipe portion and a lower portion of the large-diameter pipe portion communicate with each other for ventilation, and a nickel plating layer having a plating thickness of 0.5 to 10 μm is formed on an inner surface of at least the small-diameter pipe portion.