The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 03, 2015

Filed:

Sep. 11, 2009
Applicants:

Hidehiro Yamaguchi, Tokyo, JP;

Shigeki Yamamoto, Tokyo, JP;

Tomohiro Iko, Tokyo, JP;

Wei LI, Tokyo, JP;

Inventors:

Hidehiro Yamaguchi, Tokyo, JP;

Shigeki Yamamoto, Tokyo, JP;

Tomohiro Iko, Tokyo, JP;

Wei Li, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08G 18/02 (2006.01); C23C 28/00 (2006.01); B32B 7/12 (2006.01); B32B 15/08 (2006.01); C08G 18/08 (2006.01); C08G 18/12 (2006.01); C08G 18/32 (2006.01); C08G 18/42 (2006.01); C08G 18/66 (2006.01); C08G 18/73 (2006.01); C08G 18/75 (2006.01); C09D 5/08 (2006.01); C09J 175/04 (2006.01); B05D 5/10 (2006.01); B05D 7/14 (2006.01);
U.S. Cl.
CPC ...
C23C 28/00 (2013.01); B32B 7/12 (2013.01); B32B 15/08 (2013.01); C08G 18/0809 (2013.01); C08G 18/0814 (2013.01); C08G 18/12 (2013.01); C08G 18/3275 (2013.01); C08G 18/4213 (2013.01); C08G 18/4222 (2013.01); C08G 18/4238 (2013.01); C08G 18/6655 (2013.01); C08G 18/73 (2013.01); C08G 18/755 (2013.01); C08G 18/757 (2013.01); C08G 18/758 (2013.01); C09D 5/08 (2013.01); C09J 175/04 (2013.01); B05D 5/10 (2013.01); B05D 7/14 (2013.01); B32B 2605/00 (2013.01); C08G 2170/80 (2013.01);
Abstract

A composition for adhesion layer that is used for obtaining a multi-layered surface treatment steel sheet in which an adhesion layer is formed onto at least one surface of the steel sheet, and an upper layer and/or an intermediate layer which has a design and which contains a rust preventive pigment and/or a colored pigment is formed onto the adhesion layer; the composition including a cationic urethane resin and a silicon compound in an aqueous medium, and the ratio between the temperature at which the logarithmic decrement for the mixture of the cationic urethane resin and the silicon compound in the rigid-body pendulum type free damped vibration method shows the maximum value and the temperature at which the logarithmic decrement for the cationic urethane resin alone in the rigid-body pendulum type free damped vibration method shows the maximum value is in the range of 1.2 to 3.0.