The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Nov. 03, 2015

Filed:

Nov. 04, 2011
Applicants:

Shoichi Yamauchi, Kanagawa, JP;

Isao Yamashita, Kanagawa, JP;

Koji Tsukuma, Kanagawa, JP;

Inventors:

Shoichi Yamauchi, Kanagawa, JP;

Isao Yamashita, Kanagawa, JP;

Koji Tsukuma, Kanagawa, JP;

Assignee:

TOSOH CORPORATION, Yamaguchi, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/486 (2006.01); C04B 35/49 (2006.01); C04B 35/488 (2006.01); C04B 35/645 (2006.01);
U.S. Cl.
CPC ...
C04B 35/49 (2013.01); C04B 35/486 (2013.01); C04B 35/488 (2013.01); C04B 35/6455 (2013.01); C04B 2235/3224 (2013.01); C04B 2235/3225 (2013.01); C04B 2235/3232 (2013.01); C04B 2235/3237 (2013.01); C04B 2235/3239 (2013.01); C04B 2235/3241 (2013.01); C04B 2235/3262 (2013.01); C04B 2235/3272 (2013.01); C04B 2235/3275 (2013.01); C04B 2235/3279 (2013.01); C04B 2235/3281 (2013.01); C04B 2235/5409 (2013.01); C04B 2235/652 (2013.01); C04B 2235/656 (2013.01); C04B 2235/6565 (2013.01); C04B 2235/661 (2013.01); C04B 2235/663 (2013.01); C04B 2235/762 (2013.01); C04B 2235/77 (2013.01); C04B 2235/786 (2013.01); C04B 2235/80 (2013.01); C04B 2235/96 (2013.01); C04B 2235/963 (2013.01); C04B 2235/9653 (2013.01); C04B 2235/9661 (2013.01);
Abstract

A colored translucent zirconia sintered body contains a transition metal element as a coloring agent, having a clear color tone and high transparency, and being excellent in both design properties and esthetic properties, and its production process. A colored translucent zirconia sintered body includes yttria in an amount of at least 6 mol % and at most 15 mol % and at least one member selected from the group consisting of iron, nickel, manganese, cobalt, chromium, copper and vanadium in an amount of at least 0.02 mol % and at most 0.5 mol % as calculated as oxides, and having a porosity of at most 1,000 ppm. The average crystal grain size is preferably at most 60 μm.