The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 13, 2015

Filed:

Nov. 02, 2010
Applicants:

Zhu Ji, Tianjin, CN;

Jinsong Wang, Tianjin, CN;

Zhong Zhang, Tianjin, CN;

Yuqing Yang, Tianjin, CN;

Aishan Wang, Tianjin, CN;

Weiguo Song, Tianjin, CN;

Xinjian Yin, Tianjin, CN;

Qingting Wei, Tianjin, CN;

Hongwei RU, Tianjin, CN;

Wenwen Zhang, Tianjin, CN;

Haijun Mei, Tianjin, CN;

Inventors:

Zhu Ji, Tianjin, CN;

Jinsong Wang, Tianjin, CN;

Zhong Zhang, Tianjin, CN;

Yuqing Yang, Tianjin, CN;

Aishan Wang, Tianjin, CN;

Weiguo Song, Tianjin, CN;

Xinjian Yin, Tianjin, CN;

Qingting Wei, Tianjin, CN;

Hongwei Ru, Tianjin, CN;

Wenwen Zhang, Tianjin, CN;

Haijun Mei, Tianjin, CN;

Attorneys:
Primary Examiner:
Int. Cl.
CPC ...
C22B 34/32 (2006.01); C01G 37/14 (2006.01); C01G 49/02 (2006.01);
U.S. Cl.
CPC ...
C22B 34/32 (2013.01); C01G 37/14 (2013.01); C01G 49/02 (2013.01);
Abstract

The present invention provides a hydrothermal oxidation method for producing alkali metal dichromate from carbon ferrochrome, and the method comprises the following steps: formulating an initial reaction liquid by mixing carbon ferrochrome, an alkaline substance and water, in which the actual addition amount of the alkali is controlled smaller than the theoretically required amount; adding the initial reaction liquid into a reaction kettle, charging an oxidizing gas into the reaction kettle, and allowing the reaction to proceed for 0.5 to 3 h at a temperature of 150° C. to 370° C. and a pressure of 2 Mpa to 24 MPa; carrying out solid-liquid separation, cooling the resultant filtrate to a temperature of −12° C. to −20° C. to precipitate crystals, and carrying out separation by centrifuge to obtain alkali metal dichromate solution; adding CrOto the alkali metal dichromate solution until the degree of acidification reaches 100% or greater, concentrating the solution by evaporation, and cooling it to precipitate crystals, so as to afford alkali metal dichromate. The method has a simple process, is easy to control, and can directly produce sodium dichromate under hydrothermal conditions.


Find Patent Forward Citations

Ji, Zhu. (2015). Hydrothermal oxidation method for production of alkali metal dichromate from carbon ferrochrome (U.S. Patent No. 9157133). U.S. Patent and Trademark Office. https://idiyas.com/patent/badge/9157133

Data source: USPTO (United States Patent and Trademark Office) public patent records. Weekly synchronization. How IDiyas builds this profile

Loading…