The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Oct. 06, 2015

Filed:

May. 02, 2014
Applicant:

General Electric Company, Schenectady, NY (US);

Inventors:

Weijun Yin, Niskayuna, NY (US);

Kevin Warner Flanagan, Troy, NY (US);

Robert Colin McTigue, Coeymans Hollow, NY (US);

James Jun Xu, Niskayuna, NY (US);

Mark Edwin Rodda, Newbury Park, CA (US);

Sergei Kniajanski, Clifton Park, NY (US);

Assignee:

General Electric Company, Niskayuna, NY (US);

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C08K 9/06 (2006.01); H01F 41/06 (2006.01); H01B 3/00 (2006.01); H01B 7/29 (2006.01); H01B 3/30 (2006.01);
U.S. Cl.
CPC ...
H01F 41/0616 (2013.01); H01B 3/006 (2013.01); H01B 3/306 (2013.01); H01B 7/29 (2013.01); C08K 9/06 (2013.01); Y10T 428/2995 (2015.01); Y10T 428/31681 (2015.04);
Abstract

A method of making a composite magnet wire includes mixing alumina nano particles with a polyimide polymer to form a polyimide mixture, the alumina nano particles having a surface treatment applied to outer surfaces of the alumina nano particles, the surface treatment including a phenyl-silane; coating a wire with the polyimide mixture by passing the wire through a coating die; heating the coated wire; cooling the coated wire; passing the coated wire through an annealing oven at a temperature of about 425° C. to about 475° C. at a speed of about 15 to about 30 feet per minute to anneal the coated wire; cooling the annealed coating wire; spooling the coated wire onto a metal spool; heating the spooled wire at about 300° C. to about 400° C. for about 20 to about 40 minutes; and cooling the heated spooled wire.