The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 29, 2015

Filed:

Dec. 19, 2012
Applicants:

Sumitomo Electric Industries, Ltd., Osaka-shi, Osaka, JP;

Autonetworks Technologies, Ltd., Yokkaichi-shi, Mie, JP;

Sumitomo Wiring Systems, Ltd., Yokkaichi-shi, Mie, JP;

Sumitomo Electric Toyama Co., Ltd., Imizu-shi, Toyama, JP;

Inventors:

Misato Kusakari, Osaka, JP;

Yoshihiro Nakai, Osaka, JP;

Taichirou Nishikawa, Osaka, JP;

Yoshiyuki Takaki, Osaka, JP;

Yasuyuki Ootsuka, Yokkaichi, JP;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
H01B 1/02 (2006.01); C22C 21/00 (2006.01); B21C 1/00 (2006.01); C22F 1/00 (2006.01); C22F 1/02 (2006.01); C22F 1/04 (2006.01);
U.S. Cl.
CPC ...
H01B 1/023 (2013.01); B21C 1/00 (2013.01); C22C 21/00 (2013.01); C22F 1/00 (2013.01); C22F 1/02 (2013.01); C22F 1/04 (2013.01);
Abstract

An aluminum alloy, an aluminum alloy wire, an aluminum alloy stranded wire, a covered electric wire, and a wire harness that are of high toughness and high electrical conductivity, and a method of manufacturing an aluminum alloy wire are provided. The aluminum alloy wire contains not less than 0.005% and not more than 2.2% by mass of Fe, and a remainder including Al and an impurity. It may further contain not less than 0.005% and not more than 1.0% by mass in total of at least one additive element selected from Mg, Si, Cu, Zn, Ni, Mn, Ag, Cr, and Zr. The Al alloy wire has an electrical conductivity of not less than 58% IACS and an elongation of not less than 10%. The Al alloy wire is manufactured through the successive steps of casting, rolling, wiredrawing, and softening treatment. The softening treatment can be performed to provide an excellent toughness such as elongation and impact resistance and thereby reduce fracture of the electric wire in the vicinity of a terminal portion when the wire harness is installed.