The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 08, 2015

Filed:

Jul. 22, 2010
Applicants:

Shinsuke Ide, Tokyo, JP;

Tomohiro Ishii, Tokyo, JP;

Naoki Nishiyama, Tokyo, JP;

Shin Ishikawa, Tokyo, JP;

Takumi Ujiro, Tokyo, JP;

Noriko Makiishi, Tokyo, JP;

Inventors:

Shinsuke Ide, Tokyo, JP;

Tomohiro Ishii, Tokyo, JP;

Naoki Nishiyama, Tokyo, JP;

Shin Ishikawa, Tokyo, JP;

Takumi Ujiro, Tokyo, JP;

Noriko Makiishi, Tokyo, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 2/16 (2006.01); C25D 11/34 (2006.01); C25D 3/04 (2006.01); H01M 8/02 (2006.01); C22C 38/00 (2006.01); C22C 38/02 (2006.01); C22C 38/04 (2006.01); C22C 38/06 (2006.01); C22C 38/26 (2006.01); C22C 38/44 (2006.01); H01M 8/08 (2006.01); H01M 8/10 (2006.01); H01M 8/12 (2006.01); H01M 8/14 (2006.01);
U.S. Cl.
CPC ...
H01M 8/021 (2013.01); C22C 38/001 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); C22C 38/26 (2013.01); C22C 38/44 (2013.01); C25D 11/34 (2013.01); H01M 8/083 (2013.01); H01M 8/086 (2013.01); H01M 2008/1095 (2013.01); H01M 2008/1293 (2013.01); H01M 2008/147 (2013.01); Y02E 60/50 (2013.01); Y02E 60/525 (2013.01); Y02E 60/526 (2013.01);
Abstract

A stainless steel for a fuel cell having good corrosion resistance throughout a wide potential range and a method for producing the same are provided. In particular, a coating having an intensity ratio [(OO/OH)/(Cr/Fe)] of 1.0 or more determined by X-ray photoelectron spectroscopy analysis is formed by performing an anodic electrolyzation treatment on a surface of a stainless steel in an electrolyte solution, the stainless steel containing 16% by mass or more of Cr and preferably having a composition that includes, in terms of percent by mass, C: 0.03% or less, Si: 1.0% or less, Mn: 1.0% or less, S: 0.01% or less, P: 0.05% or less, Al: 0.20% or less, N: 0.03% or less, Cr: 20 to 40%, at least one selected from Nb, Ti, and Zr, in total: 1.0% or less, and the balance being Fe and unavoidable impurities.