The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Sep. 08, 2015

Filed:

Dec. 06, 2010
Applicants:

Satoshi Nagao, Gotenba, JP;

Kimiyasu Ono, Susono, JP;

Hirohito Hirata, Sizuoka-ken, JP;

Akihiko Suda, Seto, JP;

Kimitoshi Sato, Inazawa, JP;

Kae Yamamura, Nagoya, JP;

Akira Morikawa, Nagoya, JP;

Inventors:

Satoshi Nagao, Gotenba, JP;

Kimiyasu Ono, Susono, JP;

Hirohito Hirata, Sizuoka-ken, JP;

Akihiko Suda, Seto, JP;

Kimitoshi Sato, Inazawa, JP;

Kae Yamamura, Nagoya, JP;

Akira Morikawa, Nagoya, JP;

Assignee:
Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
B01J 23/10 (2006.01); B01J 23/00 (2006.01); B01J 23/08 (2006.01); C01F 17/00 (2006.01); B82Y 30/00 (2011.01); C01F 7/02 (2006.01); C01F 7/34 (2006.01);
U.S. Cl.
CPC ...
C01F 17/0043 (2013.01); B82Y 30/00 (2013.01); C01F 7/02 (2013.01); C01F 7/34 (2013.01); C01P 2004/52 (2013.01); C01P 2004/64 (2013.01); C01P 2004/82 (2013.01); C01P 2006/12 (2013.01);
Abstract

A method of synthesizing metal composite oxide, the method including: a step of separately introducing into a high-speed stirring apparatus a ceria composite oxide microparticle colloid having a mean particle diameter of 10 nm or less after adding a dispersant and an alumina microparticle colloid having a mean particle diameter of 10 nm or less after adding a dispersant; a step of synthesizing alumina-ceria composite oxide microparticles by allowing the ceria composite oxide microparticles and the alumina microparticles that have been introduced into the high-speed stirring apparatus to react in a microscopic space; and a step of applying a shearing force of 17000 secor more to the alumina-ceria composite oxide microparticles.