The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Aug. 11, 2015

Filed:

Jul. 10, 2011
Applicants:

Thorsten Butz, Buchholz, DE;

Matthias Nölting, Hamburg, DE;

Gunnar Winkelmann, Glinde, DE;

Inventors:

Thorsten Butz, Buchholz, DE;

Matthias Nölting, Hamburg, DE;

Gunnar Winkelmann, Glinde, DE;

Assignees:

SASOL WAX GmBH, Hamburg, DE;

STORIMPEX IM-UND EXPORT GmBH, Glinde, DE;

Attorney:
Primary Examiner:
Assistant Examiner:
Int. Cl.
CPC ...
C08L 95/00 (2006.01); C08L 21/00 (2006.01); C08J 3/12 (2006.01); C08L 17/00 (2006.01); E01C 7/26 (2006.01); C08L 91/06 (2006.01);
U.S. Cl.
CPC ...
C08L 95/00 (2013.01); C08J 3/12 (2013.01); C08J 3/128 (2013.01); C08L 17/00 (2013.01); C08L 21/00 (2013.01); E01C 7/265 (2013.01); C08J 2317/00 (2013.01); C08J 2491/06 (2013.01); C08L 91/06 (2013.01); C08L 2555/22 (2013.01); C08L 2555/52 (2013.01); C08L 2555/72 (2013.01); C08L 2555/86 (2013.01); Y10T 428/2998 (2015.01);
Abstract

A method for producing bulk good of agglomerates made of rubber particles and wax. A composition of the agglomerate and the use of the bulk good to produce asphalt or bitumen masses are created in that rubber is activated by swelling and using a swelling agent and a melt made of viscosity-reducing wax and of optional polyoctenamer is added, the activated rubber particles are agglomerated by means of the viscosity-reducing wax and optional adhesion-improving substances. The resulting larger volume leads to a viscosity reduction and the softening leads to a more intimate and more homogeneous wetting with the wax and, in the mixed good to be produced, a viscosity reduction remaining stable in the mixed good for <180 min and an increased stability of the cross-linking of the rubber molecules among each other after the agglomerates have been incorporated are achieved.