The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2015

Filed:

Jul. 13, 2009
Applicant:

Hideki Oki, Susono, JP;

Inventor:

Hideki Oki, Susono, JP;

Assignee:
Attorney:
Primary Examiner:
Int. Cl.
CPC ...
H01M 4/505 (2010.01); H01M 4/525 (2010.01); C23C 14/08 (2006.01); C23C 14/58 (2006.01); H01M 4/04 (2006.01); H01M 4/131 (2010.01); H01M 10/0562 (2010.01); H01M 4/02 (2006.01);
U.S. Cl.
CPC ...
H01M 4/505 (2013.01); C23C 14/08 (2013.01); C23C 14/5806 (2013.01); H01M 4/0423 (2013.01); H01M 4/0471 (2013.01); H01M 4/131 (2013.01); H01M 4/525 (2013.01); H01M 10/0562 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01); Y02E 60/122 (2013.01);
Abstract

The main object of the present invention is to provide a method for producing a cathode active material layer, which allows a high-purity lithium complex oxide by restraining impurities from being produced, allows a flat film, and allows orientation control. The present invention solves the above-mentioned problems by providing a method for producing a cathode active material layer, in which a cathode active material layer is formed on a substrate and contains LiXO(X is a transition metal element of at least one kind selected from the group consisting of Co, Ni and Mn, a=0.7-1.3, and b=1.5-2.5), characterized in that the method comprises the steps of: forming a cathode active material precursor-film on the above-mentioned substrate by a physical vapor deposition method while setting a temperature of the substrate at 300° C. or less, and performing an annealing treatment for the cathode active material precursor-film at a temperature of a crystallizable temperature of the LiXOor more, and characterized in that the substrate has orientation property in a surface.