The patent badge is an abbreviated version of the USPTO patent document. The patent badge does contain a link to the full patent document.

The patent badge is an abbreviated version of the USPTO patent document. The patent badge covers the following: Patent number, Date patent was issued, Date patent was filed, Title of the patent, Applicant, Inventor, Assignee, Attorney firm, Primary examiner, Assistant examiner, CPCs, and Abstract. The patent badge does contain a link to the full patent document (in Adobe Acrobat format, aka pdf). To download or print any patent click here.

Date of Patent:
Jul. 28, 2015

Filed:

Nov. 24, 2010
Applicants:

Tomoaki Karaki, Imizu, JP;

Fan Zhang, Heping District, CN;

Inventors:

Tomoaki Karaki, Imizu, JP;

Fan Zhang, Heping District, CN;

Assignees:

TOYAMA PREFECTURE, Toyama, JP;

HITACHI METALS, LTD., Tokyo, JP;

Attorney:
Primary Examiner:
Int. Cl.
CPC ...
C04B 35/495 (2006.01); C01G 33/00 (2006.01); C04B 35/626 (2006.01); H01L 41/187 (2006.01); H01L 41/43 (2013.01);
U.S. Cl.
CPC ...
C04B 35/495 (2013.01); C01G 33/006 (2013.01); C04B 35/62675 (2013.01); H01L 41/1873 (2013.01); H01L 41/43 (2013.01); C01P 2002/72 (2013.01); C01P 2002/76 (2013.01); C01P 2002/77 (2013.01); C01P 2002/88 (2013.01); C01P 2004/03 (2013.01); C01P 2004/04 (2013.01); C01P 2004/62 (2013.01); C04B 2235/3201 (2013.01); C04B 2235/3251 (2013.01); C04B 2235/3255 (2013.01); C04B 2235/5292 (2013.01); C04B 2235/5296 (2013.01); C04B 2235/5436 (2013.01); C04B 2235/768 (2013.01); C04B 2235/787 (2013.01); Y10T 428/2982 (2015.01);
Abstract

There is provided an anisotropically shaped powder preferred as plate-like crystals used in the process of producing niobate-based KNbO—NaNbO—LiNbO-based crystal-oriented ceramics and the like, and a method for producing the same. The production method includes, an oxide powder, such as NbO, and a surfactant are added to an aqueous solution of alkali hydroxides, such as NaOH and KOH to perform hydrothermal synthesis, the product obtained after this reaction is washed with an organic solvent, and further, the product after the washing is fired at 170° C. to 700° C. In addition, according to this production method, it is possible to obtain an anisotropically shaped powder having a ratio of an average particle length in a major axis direction to an average particle length in a thickness direction in the range of 2 to 20 and having a pseudo-cubic perovskite structure in which a crystal face is oriented in a (100) plane.